Journal of Peking University(Health Sciences) ›› 2015, Vol. 47 ›› Issue (6): 1005-1009. doi: 10.3969/j.issn.1671167X.2015.06.021

• Article • Previous Articles     Next Articles

Comparative research for micro-push-out bond strengths of glass fiber posts treated by poly-dopamine or silane coupling agent

CHEN Qian1*, SU Yong-liang2*, CAI Qing3, BAI Yun-yang4, SU Jing3, WANG Xin-zhi4△   

  1. (1.Second Clinical Division, Peking University School and Hospital of Stomatology, Beijing 100101, China; 2.First Clinical Division, Peking University School and Hospital of Stomatology, Beijing 100034, China; 3.State Key Laboratory of Organicinorganic Composites, Beijing University of Chemical Technology, Beijing 100029, China; 4.Department of Prosthodontics, Peking University School and Hospital of Stomatology, Beijing 100081,China)
  • Online:2015-12-18 Published:2015-12-18
  • Contact: WANG Xin-zhi E-mail:xinzwang@sina.com.cn
  • Supported by:

    Supported by National High Technology Research and Development Program of China (863 proqram, 2011AA030102) and Program for New Century Excellent Talents in University(NCET-11-0556)

Abstract:

Objective: To evaluate the micro-push-out bond strengths of prefabricated glass fiber posts with poly-dopamine functionalized to root dentin using resin cements, contrasted with silane treatment. Methods: In the study, 30 glass fiber posts were randomly divided into 3 groups (10 posts in each group) for different surface treatments. Group 1, treated with poly-dopa; Group 2, treated with silane coupling agent for 60s; Group 3, no surface treatment (Control group). The 30 extracted human, single-rooted teeth were endodontically treated and a 9 mm post space was prepared in each tooth with post drills provided by the manufacturer. Following post cementation, the specimens were stored in distilled water at 37 ℃ for 7 days. The micro-push-out bond strengths were tested using a universal testing machine (0.5 mm/min), and the failure modes were examined with a stereomicroscope. The data of the three groups were statistically analyzed using the one-way ANOVA test(α= 0.05).Results: The bond strengths were (7.909±1.987) MPa for Group 1, (5.906 ±0.620) MPa for Group 2, and 4.678 ±0.910 MPa for Group 3. The bond strength of poly-dopamine group was significantly higher than that of the silane group (P<0.05). Conclusion: Contrasted with silane treatment, surface poly-dopamine functionalization was confirmed to be a more reliable method for improving the bond strength of resin luting agents to fiber posts.

Key words: Glass fiber posts, Poly-dopamine, Silane, Push-out bond strength

CLC Number: 

  • R781.33
[1] Qian CHEN,Xin-zhi WANG. Evaluation of modified micro-push-out bond strength of glass fiber posts with chemically treated resin cements [J]. Journal of Peking University(Health Sciences), 2019, 51(5): 968-972.
[2] Yuan ZHANG,Jian-min HAN,Lin LIU,Xu-liang DENG. Study of bond strength of one-piece glass fiber posts-and-cores with flared root canals in vitro [J]. Journal of Peking University(Health Sciences), 2019, 51(2): 327-334.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!