Journal of Peking University(Health Sciences) ›› 2018, Vol. 50 ›› Issue (1): 49-52. doi: 10.3969/j.issn.1671-167X.2018.01.008

• Article • Previous Articles     Next Articles

Effect of different surface treatments on the crystal structure and properties of zirconia

JIAO Yang1, WANG Ji-de2, DENG Jiu-peng2△   

  1. (1. Department of Stomatology,Peking University First Hospital, Beijing 100034, China; 2. Department of Prosthodontics,College of Stomatology,North China University of Science and Technology, Tangshan 063000, Hebei, China)
  • Online:2018-02-18 Published:2018-02-18
  • Contact: DENG Jiu-peng E-mail:jiupeng00261@sina.com

Abstract: Objective:To investigate the effects of 3 surface different treatments on the crystal structure, shear bond strength,roughness value and flexural strength of zirconia. Methods: The zirconia spe-cimens were prepared and randomly divided into 4 groups and received the following treatments: (1)blank control group,the specimens without treatments; (2)sandblasting with alumina group, sandblasting the specimens with 110 μm alumina particles for 21 s as working pressure 0.25 MPa and working distance 10 mm; (3)laser etching group, coating the surface of the specimens with graphite powder and using Er:Yttrium Aluminum Garnet (Er:YAG) laser to irradiate the surface 30 s; (4) hot-etching group, putting the specimens in a closed reactor within a 1 ∶1 mixture of 40%(mass traction) nitric acid and 68%(mass traction) hydrofluoric acid liquid, the reaction of 30 min in a water bath at 100 degrees centigrade. The changes of crystal structure, shear bond strength(SBS) and flexural strength of zirconia after different surface treatments were tested. Results: The X-ray diffractometer(XRD) patterns showed that the volume percentage of monoclinic phase of the 4 groups was 0.91%, 12.50%, 6.64% and 17.81% respectively. The roughness value for the four groups  were as follows: blank control group,(0.29±0.01) μm; sandblasting with alumina group, (1.05±0.11) μm; laser etching group, (0.73±0.04) μm; hot-etching group, (1.31±0.06) μm, respectively(P<0.05). Mean SBS was (7.09±0.46) MPa in blank control group, (12.14±1.51) MPa in sandblasting with alumina group, (8.82±0.74) MPa in laser etching group and (11.97±0.99) MPa in hot-etching group. There was no statistically significant difference between sandblasting with alumina group and hot-etching group (P>0.05), but the difference between the other groups were statistically significant(P<0.05). Mean three-point bending was (933.70±44.13) MPa in blank control group, (850.95±60.66) MPa in sandblasting with alumina group, (771.53±68.08) MPa in laser etching group and (766.27±57.49) MPa in hot-etching group. There was no statistically significant difference between sandblasting with alumina group and hot-etching group (P>0.05), but the difference between the other groups were statistically significant(P<0.05). Conclusion: After different surface treatments, the surface of zirconia has changed from tetrago-nal to monoclinic phases in varying degrees. In addition, surface treatments could improve the bond strength of zirconia to resin cement, and also lead to a decrease in the flexural strength of zirconia.

Key words: Zirconia, Sandblasted, Hot-etching

CLC Number: 

  •  
[1] WANG Zheng,DING Qian,GAO Yuan,MA Quan-quan,ZHANG Lei,GE Xi-yuan,SUN Yu-chun,XIE Qiu-fei. Effect of porous zirconia ceramics on proliferation and differentiation of osteoblasts [J]. Journal of Peking University (Health Sciences), 2022, 54(1): 31-39.
[2] LI Wen-jin,DING Qian,YUAN Fu-song,Sun Feng-bo,ZHENG Jian-qiao,BAO Rui,Zhang Lei. Effects of femtosecond laser treatment on surface characteristics and flexural strength of zirconia [J]. Journal of Peking University (Health Sciences), 2021, 53(4): 770-775.
[3] YANG Xin,LI Rong,YE Hong-qiang,CHEN Hu,WANG Yong,ZHOU Yong-sheng,SUN Yu-chun. Evaluation of fracture strength of two kinds of zirconia all-ceramic crowns with different edge compensation angles [J]. Journal of Peking University (Health Sciences), 2021, 53(2): 402-405.
[4] Miao ZHENG,Ling-lu ZHAN,Zhi-qiang LIU,He-ping LI,Jian-guo TAN. Effect of different plasma treated zirconia on the adhensive behaviour of human gingival fibroblasts [J]. Journal of Peking University(Health Sciences), 2019, 51(2): 315-320.
[5] ZHOU Tuan-feng, WANG Xin-zhi . Clinical observation of the restoration of computer aided designed and manufactured one-piece zirconia posts and cores: a 5-year prospective follow-up study [J]. Journal of Peking University(Health Sciences), 2018, 50(4): 680-684.
[6] CUI Xin-yue, TONG Dai, WANG Xin-zhi, SHEN Zhi-jian. Comparison of the translucency and color masking effect of the zirconia ceramics made by milling and gel deposition [J]. Journal of Peking University(Health Sciences), 2018, 50(1): 85-90.
[7] LIAO Yu, LIU Xiao-qiang, CHEN Li, ZHOU Jian-feng, TAN Jian-guo. Effects of different surface treatments on the zirconia-resin cement bond strength [J]. Journal of Peking University(Health Sciences), 2018, 50(1): 53-57.
[8] ZHOU Tuan-Feng, ZHANG Xiang-Hao, WANG Xin-Zhi. Three-dimensional finite element analysis of one-piece computer aided design and computer aided manufacture involved zirconia post and core [J]. Journal of Peking University(Health Sciences), 2015, 47(1): 78-84.
[9] 吕Pin , JIANG Ting. Effect of surface hot-etching treatment on zirconia/resin bonding strength [J]. Journal of Peking University(Health Sciences), 2014, 46(2): 302-305.
[10] LIU Yi-hong, WANG Yong, ZHANG Qing-hui, GAO Yuan, FENG Hai-lan. Fracture reliability of zirconia all-ceramic crown according to zirconia coping design [J]. Journal of Peking University(Health Sciences), 2014, 46(1): 71-75.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
[1] . [J]. Journal of Peking University(Health Sciences), 2009, 41(4): 456 -458 .
[2] . [J]. Journal of Peking University(Health Sciences), 2009, 41(2): 125 -128 .
[3] . [J]. Journal of Peking University(Health Sciences), 2009, 41(2): 135 -140 .
[4] . [J]. Journal of Peking University(Health Sciences), 2009, 41(2): 158 -161 .
[5] . [J]. Journal of Peking University(Health Sciences), 2009, 41(2): 217 -220 .
[6] . [J]. Journal of Peking University(Health Sciences), 2009, 41(1): 52 -55 .
[7] . [J]. Journal of Peking University(Health Sciences), 2009, 41(1): 109 -111 .
[8] . [J]. Journal of Peking University(Health Sciences), 2009, 41(3): 297 -301 .
[9] . [J]. Journal of Peking University(Health Sciences), 2009, 41(5): 599 -601 .
[10] . [J]. Journal of Peking University(Health Sciences), 2009, 41(5): 516 -520 .